Signoff

Sample questions › General

Cleaning and Corrosion Control

20 of Signoff's 67 oral practice questions for this subject (General, ACS AM.I.G). Say your answer out loud first, then check it against the FAA's own words.

Practice these out loud. In the Signoff app an examiner voice asks, you answer by voice or typing, and every key point is checked against the cited answer. See how it works.

Why should an aircraft be washed in the shade whenever possible?

Cleaning compounds tend to streak the surface if they are applied to hot metal or allowed to dry on it.

What the examiner wants to hear

“The washing of aircraft should be performed in the shade whenever possible, as cleaning compounds tend to streak the surface if applied to hot metal or are permitted to dry on the area.”FAA-H-8083-30B, General Handbook, p. 8-24

ACS AM.I.G.K1

When rinsing stripper residue from a surface, what water pressure does the handbook recommend, and what precaution applies when wet washing an aircraft?

Use a low to medium pressure water stream on the area being scrubbed. Before washing, install covers over openings where water or cleaners could enter and cause damage.

What the examiner wants to hear

“If water spray is available, use a low to medium pressure stream of water directly on the area being scrubbed.”FAA-H-8083-30B, General Handbook, p. 8-15
“Install covers over all openings where water or cleaners might enter and cause damage.”FAA-H-8083-30B, General Handbook, p. 8-24

ACS AM.I.G.K10

Why must cleaners used on aluminum be chosen carefully?

Alkaline or caustic cleaners that are not fully rinsed and neutralized can cause corrosion in lap joints; many consumer products are caustic enough to do this, so choose a neutral pH product.

What the examiner wants to hear

“As mentioned previously, cleaners that can be effectively rinsed and neutralized must be used, or an alkaline cleaner may cause corrosion within the lap joints of riveted or spot-welded sheet metal components.”FAA-H-8083-30B, General Handbook, p. 8-23
“Many commercial consumer products are actually caustic enough to induce corrosion if trapped between aluminum lap joints. Choose a neutral pH product.”FAA-H-8083-30B, General Handbook, p. 8-18

ACS AM.I.G.K11

What determines the rate of galvanic corrosion?

The difference in activity between the metals: the greater the difference, the faster the corrosion. Also relative size: if the corroding metal is smaller than the less active metal, corrosion is rapid and severe.

What the examiner wants to hear

“The greater the difference in activity, the faster corrosion occurs. The rate of galvanic corrosion also depends on the size of the parts in contact. If the surface area of the corroding metal is smaller than the surface area of the less active metal, corrosion is rapid and severe. When the corroding metal is larger than the less active metal, corrosion is slow and superficial.”FAA-H-8083-30B, General Handbook, p. 8-10

ACS AM.I.G.K12

What is alodizing, and why is it used?

A simple chemical treatment for all aluminum alloys that increases their corrosion resistance and improves paint bonding.

What the examiner wants to hear

“Alodizing is a simple chemical treatment for all aluminum alloys to increase their corrosion resistance and to improve their paint bonding qualities. Because of its simplicity, it is rapidly replacing anodizing in aircraft work.”FAA-H-8083-30B, General Handbook, p. 8-22

ACS AM.I.G.K13

What is Alclad, and how does it protect the core alloy?

Sheet with an aluminum-alloy core coated with pure aluminum about 5 1⁄2 percent deep on each side. The pure aluminum keeps corrosive agents from the core and protects it electrolytically.

What the examiner wants to hear

“The terms "Alclad and Pureclad" are used to designate sheets that consist of an aluminum-alloy core coated with a layer of pure aluminum to a depth of approximately 51⁄2 percent on each side. The pure aluminum coating affords a dual protection for the core, preventing contact with any corrosive agents, and protecting the core electrolytically by preventing”FAA-H-8083-30B, General Handbook, p. 7-21

ACS AM.I.G.K14

If a protective coating must be applied to a rivet on the job, what is done?

Paint the rivet with zinc chromate before it is used and again after it is driven.

What the examiner wants to hear

“If a situation arises in which a protective coating must be applied on the job, paint the rivet with zinc chromate before it is used and again after it is driven.”FAA-H-8083-30B, General Handbook, p. 7-54

ACS AM.I.G.K15

What are the most common protective paint finishes on aircraft?

Catalyzed polyurethane enamel, waterborne polyurethane enamel, and two-part epoxy paint; waterborne systems are increasing because of VOC regulations.

What the examiner wants to hear

“The most common finishes include catalyzed polyurethane enamel, waterborne polyurethane enamel, and two-part epoxy paint. As new regulations regarding the emission of volatile organic compounds (VOCs) are put into effect, the use of waterborne paint systems have increased in popularity.”FAA-H-8083-30B, General Handbook, p. 8-23

ACS AM.I.G.K16

Why are aluminum parts anodized or alodized before painting, and is an Alclad surface anodized?

The anodic coating is an excellent bond for paint. Alclad left unpainted needs no anodizing, but Alclad to be painted is usually anodized for paint bonding.

What the examiner wants to hear

“In addition to its corrosion resistant qualities, the anodic coating is also an excellent bond for paint.”FAA-H-8083-30B, General Handbook, p. 8-22
“Alclad surfaces that are to be left unpainted require no anodic treatment; however, if the Alclad surface is to be painted, it is usually anodized to provide a bond for the paint.”FAA-H-8083-30B, General Handbook, p. 8-22

ACS AM.I.G.K17

Under what ambient conditions does filiform corrosion form under paint, and how is it prevented?

It occurs when relative humidity is between 78 and 90 percent and the surface is slightly acidic. Prevent it by storing aircraft below 70 percent relative humidity, using low-diffusion coatings, and washing off acidic contaminants.

What the examiner wants to hear

“Filiform occurs when the relative humidity of the air is between 78–90 percent, and the surface is slightly acidic.”FAA-H-8083-30B, General Handbook, p. 8-5
“Filiform corrosion can be prevented by storing aircraft in an environment with a relative humidity below 70 percent, using coating systems having a low rate of diffusion for oxygen and water vapors, and by washing the aircraft to remove acidic contaminants from the surface, such as those created by pollutants in the air.”FAA-H-8083-30B, General Handbook, p. 8-6

ACS AM.I.G.K18

How can residues from chemical surface treatments affect a paint finish?

Soluble salts from treatments such as chromic acid or dichromate liquefy and promote blistering in the paint, so all residues must be removed. When treating magnesium, excess chromic acid solution left to dry on the surface causes paint lifting.

What the examiner wants to hear

“It is emphasized that all residues must be removed. Soluble salts from chemical surface treatments, such as chromic acid or dichromate treatment, liquefy and promote blistering in the paint coatings.”FAA-H-8083-30B, General Handbook, p. 8-29
“Do not allow the excess solution to dry and remain on the surface, as paint lifting is caused by such deposits.”FAA-H-8083-30B, General Handbook, p. 8-19

ACS AM.I.G.K19

What four conditions must exist for electrochemical corrosion to occur?

A metal subject to corrosion (anode), a dissimilar conductive material with less tendency to corrode (cathode), a continuous conductive liquid path, and electrical contact between anode and cathode. Removing any one stops it.

What the examiner wants to hear

“A metal subject to corrosion (anode) 2. A dissimilar conductive material (cathode) that has less tendency to corrode 3. Presence of a continuous, conductive liquid path (electrolyte) 4. Electrical contact between the anode and the cathode”FAA-H-8083-30B, General Handbook, p. 8-3
“Elimination of any one of these conditions stops electrochemical corrosion.”FAA-H-8083-30B, General Handbook, p. 8-3

ACS AM.I.G.K2

Under 14 CFR 45.11 and 45.13, what information must the fireproof identification plate on an aircraft or aircraft engine include?

The builder's name, model designation and builder's serial number, plus the type certificate and production certificate numbers if any. An engine plate also shows the established rating, and for part 34 engines the date of manufacture and an FAA-approved exhaust emission designation.

What the examiner wants to hear

“A manufacturer of aircraft covered under § 21.182 of this chapter must mark each aircraft by attaching a fireproof identification plate that— (1) Includes the information specified in § 45.13 using an approved method of fireproof marking;”14 CFR § 45.11
“A manufacturer of an aircraft engine produced under a type certificate or production certificate must mark each engine by attaching a fireproof identification plate. Such plate— (1) Must include the information specified in § 45.13 using an approved method of fireproof marking;”14 CFR § 45.11
“The identification required by § 45.11 (a) through (c) must include the following information: (1) Builder's name. (2) Model designation. (3) Builder's serial number. (4) Type certificate number, if any. (5) Production certificate number, if any. (6) For aircraft engines, the established rating. (7) On or after January 1, 1984, for aircraft engines specified in part 34 of this chapter, the date of manufacture as defined in § 34.1 of this chapter, and a designation, approved by the FAA, that indicates compliance with the applicable exhaust emission provisions of part 34 of this chapter and 40 CFR part 87.”14 CFR § 45.13

ACS AM.I.G.K20

How can corrosion spreading under a paint or plating film be recognized?

Instead of roughening or powder, the paint or plating is lifted off in small blisters caused by the pressure of corrosion products underneath.

What the examiner wants to hear

“Instead, closer inspection reveals the paint or plating is lifted off the surface in small blisters that result from the pressure of the underlying accumulation of corrosion products.”FAA-H-8083-30B, General Handbook, p. 8-5

ACS AM.I.G.K21

What hazards come with chemical surface treatment materials?

Container labels may not list every hazard, so consult the SDS; some react violently if mixed with paint thinners. Chromium trioxide is a strong oxidizer that must be stored away from organic solvents and combustibles.

What the examiner wants to hear

“However, the label might not be large enough to accommodate a list of all the possible hazards that may ensue if the materials are mixed with incompatible substances. The Safety Data Sheet (SDS) should also be consulted for information. For example, some chemicals used in surface treatments react violently if inadvertently mixed with paint thinners.”FAA-H-8083-30B, General Handbook, p. 8-22
“Chromium trioxide flake is a powerful oxidizing agent and a fairly strong acid. It must be stored away from organic solvents and other combustibles.”FAA-H-8083-30B, General Handbook, p. 8-22

ACS AM.I.G.K22

How is chemical paint stripper applied and worked?

Brush on a cover 1⁄32 to 1⁄16 inch deep, leave it until the paint wrinkles and lifts, scrub, reapply where needed, and use only nonmetallic scrapers.

What the examiner wants to hear

“Brush the entire area to be stripped with a cover of stripper to a depth of 1⁄32" to 1⁄16".”FAA-H-8083-30B, General Handbook, p. 8-15
“Allow the stripper to remain on the surface for a sufficient length of time to wrinkle and lift the paint. This may be from 10 minutes to several hours, depending on temperature, humidity, and the condition of the paint coat being removed. Scrub the surface with a bristle brush saturated with paint remover to further loosen finish that may still be adhering to the metal.”FAA-H-8083-30B, General Handbook, p. 8-15
“Reapply the stripper as necessary in areas where the paint remains tightly adhered or where the stripper has dried, and repeat the above process. Only nonmetallic scrapers are to be used to assist in removing persistent paint finishes.”FAA-H-8083-30B, General Handbook, p. 8-15

ACS AM.I.G.K23

What is filiform corrosion, and how is it recognized?

A special oxygen concentration cell under organic coatings, seen as wormlike traces of corrosion products beneath the paint. Polyurethane finishes are especially susceptible.

What the examiner wants to hear

“Filiform corrosion is a special form of oxygen concentration cell that occurs on metal surfaces having an organic coating system. It is recognized by its characteristic wormlike trace of corrosion products beneath the paint film.”FAA-H-8083-30B, General Handbook, p. 8-5
“Polyurethane finishes are especially susceptible to filiform corrosion.”FAA-H-8083-30B, General Handbook, p. 8-5

ACS AM.I.G.K3

Why are piano hinges corrosion prone, and how are they serviced?

The steel pin contacting the aluminum hinge is a dissimilar metal contact, and hinges trap dirt, salt, and moisture. Inspect, lubricate with water-displacing lubricant, and actuate through several cycles.

What the examiner wants to hear

“Piano-type hinges are prime spots for corrosion due to the dissimilar metal contact between the steel pin and aluminum hinge. They are also natural traps for dirt, salt, and moisture. Inspection of hinges must include lubrication and actuation through several cycles to ensure complete lubricant penetration. Use water-displacing lubricants when servicing piano hinges.”FAA-H-8083-30B, General Handbook, p. 8-13

ACS AM.I.G.K4

Why is keeping an aircraft clean part of corrosion prevention?

Removing the conductive medium by regular cleaning and refinishing eliminates the tiny electrical circuit, so corrosion cannot occur; this is the basis of effective corrosion control.

What the examiner wants to hear

“If, by regular cleaning and surface refinishing, the medium is removed and the minute electrical circuit eliminated, corrosion cannot occur. This is the basis for effective corrosion control.”FAA-H-8083-30B, General Handbook, p. 8-5

ACS AM.I.G.K5

Describe the steps of a corrosion inspection.

Start with a thorough cleaning, then a general inspection to find obvious defects and suspect areas, followed by a detailed inspection of those areas.

What the examiner wants to hear

“All corrosion inspections start with a thorough cleaning of the area to be inspected.”FAA-H-8083-30B, General Handbook, p. 8-11
“The general inspection is to look for obvious defects and suspected areas. A detailed inspection of damage or suspected areas found during the general inspection follows.”FAA-H-8083-30B, General Handbook, p. 8-11

ACS AM.I.G.K6